The purpose of this study was to produce poly(DL-lactic-co-glycolic acid) (PLGA) – based microparticles (MPs), externally decorated withhyaluronic acid(HA). The MPs areintended for intravitreal injections inthe treatment of posterior eye segment and have been designed to prolong the release of growth factors into the vitreous body, therefore aiming to increase the time interval between two consecutive injections. The MPs, prepared by a modified double emulsion-solvent evaporation technique and loaded with bovine serum albumins (BSA) and ciliary neurotrophic factor (CNTF), were spherical, with a diameter around 70 μm and a>90% encapsulation efficiency. Energy Dispersive Spectroscopy (EDS) outcomes indicated that HA presence in the external aqueous phase of the emulsion did affect the surface properties of MPs. Moreover, poloxamers drastically slowed down MP degradation properties which are, in turn, closely related to their ability to prolong drug release. This is promising for the envisaged application of the produced MPs. Further work will be devoted to optimizing MP formulation with respect to the envisaged intravitreal route of administration.

Electron dispersive X-ray spectroscopy and degradation properties of hyaluronic acid decorated microparticles

Frigione M.;
2019-01-01

Abstract

The purpose of this study was to produce poly(DL-lactic-co-glycolic acid) (PLGA) – based microparticles (MPs), externally decorated withhyaluronic acid(HA). The MPs areintended for intravitreal injections inthe treatment of posterior eye segment and have been designed to prolong the release of growth factors into the vitreous body, therefore aiming to increase the time interval between two consecutive injections. The MPs, prepared by a modified double emulsion-solvent evaporation technique and loaded with bovine serum albumins (BSA) and ciliary neurotrophic factor (CNTF), were spherical, with a diameter around 70 μm and a>90% encapsulation efficiency. Energy Dispersive Spectroscopy (EDS) outcomes indicated that HA presence in the external aqueous phase of the emulsion did affect the surface properties of MPs. Moreover, poloxamers drastically slowed down MP degradation properties which are, in turn, closely related to their ability to prolong drug release. This is promising for the envisaged application of the produced MPs. Further work will be devoted to optimizing MP formulation with respect to the envisaged intravitreal route of administration.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11587/431551
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 8
  • ???jsp.display-item.citation.isi??? 7
social impact