Herein, we described the synthesis of a novel ion-imprinted membrane for the detection of palladium(II) prepared through the glutaraldehyde crosslinking of chitosan with a 4-[(4-Hydroxy)phenylazo]benzenesulfonic acid ligand trapped into the membrane. The imprinting technology was used to improve adsorption capacity and adsorption selectivity, and was combined with some advantages of the developed membrane, such as low cost and ease of preparation, water-friendly synthesis, and high biocompatible chitosan material. The membranes were characterized by Fourier Transform Infrared Spectroscopy (FTIR), Scanning Electron Microscopy (SEM), and Energy Dispersive X-ray Spectrometry (EDS). The results obtained showed a high swelling ratio with a maximum value of 16.4 (1640%) at pH 4 with a strong pH dependence. Batch rebinding experiments gave a maximum adsorption capacity of 101.6 mg of Pd(II) per gram of imprinted membrane. The Pd(II) adsorption behavior was well-described by a Langmuir model with a theoretical maximum adsorption capacity of 93.48 mg g(-1), similar to the experimental one. Finally, a selectivity study versus Ag(I), Pb(II), and Fe(III) ions demonstrated a good selectivity of chitosan-imprinted membrane towards Pd(II).

A New Ion-Imprinted Chitosan-Based Membrane with an Azo-Derivative Ligand for the Efficient Removal of Pd(II)

DI BELLO, MARIA PIA;LAZZOI, MARIA ROSARIA;MELE, Giuseppe Agostino;SCORRANO, SONIA;MERGOLA, LUCIA;DEL SOLE, Roberta
2017-01-01

Abstract

Herein, we described the synthesis of a novel ion-imprinted membrane for the detection of palladium(II) prepared through the glutaraldehyde crosslinking of chitosan with a 4-[(4-Hydroxy)phenylazo]benzenesulfonic acid ligand trapped into the membrane. The imprinting technology was used to improve adsorption capacity and adsorption selectivity, and was combined with some advantages of the developed membrane, such as low cost and ease of preparation, water-friendly synthesis, and high biocompatible chitosan material. The membranes were characterized by Fourier Transform Infrared Spectroscopy (FTIR), Scanning Electron Microscopy (SEM), and Energy Dispersive X-ray Spectrometry (EDS). The results obtained showed a high swelling ratio with a maximum value of 16.4 (1640%) at pH 4 with a strong pH dependence. Batch rebinding experiments gave a maximum adsorption capacity of 101.6 mg of Pd(II) per gram of imprinted membrane. The Pd(II) adsorption behavior was well-described by a Langmuir model with a theoretical maximum adsorption capacity of 93.48 mg g(-1), similar to the experimental one. Finally, a selectivity study versus Ag(I), Pb(II), and Fe(III) ions demonstrated a good selectivity of chitosan-imprinted membrane towards Pd(II).
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11587/416424
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 29
  • ???jsp.display-item.citation.isi??? 29
social impact